Research on Flexible Sand-laying-based Precision FormingTechnology for Multimaterial Sand Molds
Author of the article:FU Haifeng1, ZHANG Xueliang2, YANG Haoqin3,4, YAN Dandan3, SHAN Zhongde3,HU Yangyang3, LI Yongjun1,
Author's Workplace:1. AECC Harbin Dongan Engine Co., Ltd., Harbin 150060, China; 2. Nanjing Changjiang Industrial Technology ResearchInstitute Co., Ltd., Nanjing 211500, China; 3. Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China;4. China Academy of Machinery Science and Technology Group Co., Ltd., Beijing 100044, China
Key Words:multimaterial sand molds; density characterization; composite performance; precise forming; accuracyverification
Abstract:
To meet the precision manufacturing requirements of multimaterial sand molds via flexible sand laying, anexperimental investigation into the multimaterial and multiregional sand laying process was carried out. With chromite sandand silica sand as the composite molding system, layer thickness errors in regional sand laying were analysed throughspecimen weight and density measurements. The sand laying accuracy, interfacial bonding behavior, and mechanicalproperties of the composite sand molds are examined, and the mechanism through which flexible regional sand layingaffects the specimen density uniformity and formability is revealed. The results demonstrate that a higher relative sandlaying density corresponds to a more uniform particle distribution, denser samples, and a more stable layer thickness anddensity. On the basis of the quantitative relationship between density and volume, the single-layer sand-laying error of thechromite sand remains within 4% of the layer thickness, and the layer thickness error for the 0.5 mm sand layer iscontrolled within ±0.02 mm. For multiregional combined sand laying in composite molds, the positional deviation error isless than 15%, and the dimensional error of the profile area is less than 25%. The tensile strength of the composite sandmold samples ranged from 1.44~1.81 MPa, and the compressive strength ranged from 4.41~5.58 MPa, which are higher than those of the single chromite sand samples and combine the performance advantages of the two molding sands.Following reliability verification of the device with optimized process parameters, multimaterial sand molds for the upperand lower molds of a gear chamber cover are successfully fabricated, and their performance is validated through castingtrials. The prepared sand molds achieve a dimensional tolerance grade of CT7, and the castings achieve grades CT8~CT9,which verifies the feasibility and precision of the proposed process.