Study on the Densification Behavior, Microstructure, and MechanicalProperties of Novel Hot-work Tool Steel Fabricated by LaserPowder Bed Fusion
Author of the article:TANG Yuanchen1,2, WU Enzhen1,2, LU Lei1, WEN Han1, LUO Wei2,XIE Xinliang1,2, WU Jiahao3, CUI Ran3
Author's Workplace:1. Key Laboratory for Light-weight Materials, Nanjing Tech University, Nanjing 211816, China; 2. Materials Academy,JITRI, Suzhou 215133, China; 3. School of Materials Science and Engineering, Tsinghua University, Beijing 100084, China
Key Words:laser powder bed fusion; hot-work tool steel; heat treatment; retained austenite; microstructure; mechanicalproperties
Abstract:
To address the severe cracking tendency and inadequate strength-toughness balance of conventional hot-worktool steels fabricated by laser powder bed fusion (LPBF), H13 and 316 L stainless steel powders were blended at a massratio of 6∶1 to achieve an in situ alloying design, reducing the C content while increasing the Ni and Cr contents. A novelcrack-free hot-work tool steel for LPBF was successfully developed. The effects of laser processing parameters ondensification were systematically investigated, and the microstructural evolution and mechanical properties of the as-built,quenched-and-double-tempered (QT2), and directly double-tempered (DT2) samples were characterized by OM, SEM,EBSD, and XRD. The results show that when the volumetric energy density exceeds 60 J/mm3, the relative density exceeds99.5%. The retained austenite contents of the as-built, QT2, and DT2 samples are 11.4%, 3.6%, and 2.6%, respectively.The DT2 sample exhibits the best overall mechanical performance, with a yield strength of 1 866 MPa, an ultimate tensilestrength of 1 974 MPa, a microhardness of 632 HV0.1, and an impact energy of 17.8 J. Direct double tempering preservesthe fine martensitic and carbide microstructures of the as-built state, thereby achieving high strength and impact toughness.